Pitch Binder
  • Product standards

    Q/640181BCXC 002—2021

  • Package

    *Canned

Technical requirement

Test itemsTechnical indicators
Softening point,℃70~100
Quinolone insoluble ,w/%8-12
Toluene insoluble ,w/%20~35
Coking value,w/%≥50
Ash content,w/%≤0.30
Moisture,w/%≤1.0

Use to

It is mainly used as binder for carbon products or road asphalt, modified asphalt, roof coating, building materials, pitch coke, carbon products and pitch forelectrodes, etc.